Sanding a vette is a hell of a job. I did mine partially and the remaining with a heat gun. My painter advised to sand with steps of 100. 80, 180, 280. But contact your painter first, mine preferred ending with 180 since there was some smoothing needed with filler. Make sure all repairs are done een smoothed out.
![[Bild: EPSN0057%20%28Medium%29.JPG]](https://lh4.ggpht.com/_W8gfKFqlA2E/RhyKxhGNFsI/AAAAAAAAATU/KAwjT-7c5js/s800/EPSN0057%20%28Medium%29.JPG)
![[Bild: DSC00909.JPG]](https://lh5.ggpht.com/_W8gfKFqlA2E/RhyKyxGNFvI/AAAAAAAAATs/wFr7QOis1PA/s800/DSC00909.JPG)
It's a very dusty job
One of the repairs needed
![[Bild: EPSN0128.JPG]](https://lh6.ggpht.com/_W8gfKFqlA2E/RhyLwBGNGpI/AAAAAAAAAa8/blDE8ghsgZ8/s800/EPSN0128.JPG)
As handed over to the professional.
![[Bild: april2008%20005.jpg]](https://lh4.ggpht.com/_W8gfKFqlA2E/SBS0ko-BA_I/AAAAAAAABTw/vU30UN1eE_8/s800/april2008%20005.jpg)
Filler
![[Bild: april2008%20008.jpg]](https://lh5.ggpht.com/_W8gfKFqlA2E/SBS0m4-BBBI/AAAAAAAABUA/nUFfXL09MPM/s800/april2008%20008.jpg)
![[Bild: april2008%20010.jpg]](https://lh6.ggpht.com/_W8gfKFqlA2E/SBS0pI-BBDI/AAAAAAAABUQ/TcQlHq4NhsA/s800/april2008%20010.jpg)
Control layer
![[Bild: april2008%20013.jpg]](https://lh3.ggpht.com/_W8gfKFqlA2E/SBS0tY-BBHI/AAAAAAAABU0/u18R4Mr4F-w/s800/april2008%20013.jpg)
Professional blocking
![[Bild: mei2008-2%20001.jpg]](https://lh5.ggpht.com/_W8gfKFqlA2E/SCytdv0SB1I/AAAAAAAABWE/ht6CVQIuJ10/s800/mei2008-2%20001.jpg)
Epoxy
![[Bild: april2008-3%20005.jpg]](https://lh5.ggpht.com/_W8gfKFqlA2E/SDclXcm8RtI/AAAAAAAABZg/p_TNCnMzZ7c/s800/april2008-3%20005.jpg)
Primer
![[Bild: april2008-3%20008.jpg]](https://lh5.ggpht.com/_W8gfKFqlA2E/SDclZcm8RwI/AAAAAAAABZ4/lLvlVk40FBc/s800/april2008-3%20008.jpg)
Base
![[Bild: 100_0543.JPG]](https://lh5.ggpht.com/_W8gfKFqlA2E/SHnjXtXNgbI/AAAAAAAABlE/RDDrea-RzMQ/s800/100_0543.JPG)
Clear
![[Bild: cas%20039.jpg]](https://lh4.ggpht.com/_W8gfKFqlA2E/SH5fiSycSSI/AAAAAAAAB5k/dXamdygzirI/s800/cas%20039.jpg)
End result
![[Bild: cas%20027.jpg]](https://lh4.ggpht.com/_W8gfKFqlA2E/SH5eNlN75CI/AAAAAAAAB4g/Vby9NkiThy8/s800/cas%20027.jpg)
![[Bild: cas%20026.jpg]](https://lh5.ggpht.com/_W8gfKFqlA2E/SH5eMf69pSI/AAAAAAAAB4Y/L3n49nTHJ00/s800/cas%20026.jpg)
Okay, now the painter can give you a more precise price when the paint is removed, no more hidden repairs.
Sand with a eccentric rotary sander, with flex plate. WEAR A AAA QUALITY DUST MASK
You can try with a heat gun and razorblade
Sand layer by layer, don't dive in there and grind to the core,
Ich habe ein paar Fotos von das lackieren von meinem 72.
Sanding a vette is a hell of a job. I did mine partially and the remaining with a heat gun. My painter advised to sand with steps of 100. 80, 180, 280. But contact your painter first, mine preferred ending with 180 since there was some smoothing needed with filler. Make sure all repairs are done een smoothed out.
It's a very dusty job
One of the repairs needed
As handed over to the professional.
![[Bild: april2008%20005.jpg]](https://lh4.ggpht.com/_W8gfKFqlA2E/SBS0ko-BA_I/AAAAAAAABTw/vU30UN1eE_8/s800/april2008%20005.jpg)
Filler
![[Bild: april2008%20008.jpg]](https://lh5.ggpht.com/_W8gfKFqlA2E/SBS0m4-BBBI/AAAAAAAABUA/nUFfXL09MPM/s800/april2008%20008.jpg)
![[Bild: april2008%20010.jpg]](https://lh6.ggpht.com/_W8gfKFqlA2E/SBS0pI-BBDI/AAAAAAAABUQ/TcQlHq4NhsA/s800/april2008%20010.jpg)
Control layer
![[Bild: april2008%20013.jpg]](https://lh3.ggpht.com/_W8gfKFqlA2E/SBS0tY-BBHI/AAAAAAAABU0/u18R4Mr4F-w/s800/april2008%20013.jpg)
Professional blocking
![[Bild: mei2008-2%20001.jpg]](https://lh5.ggpht.com/_W8gfKFqlA2E/SCytdv0SB1I/AAAAAAAABWE/ht6CVQIuJ10/s800/mei2008-2%20001.jpg)
Epoxy
![[Bild: april2008-3%20005.jpg]](https://lh5.ggpht.com/_W8gfKFqlA2E/SDclXcm8RtI/AAAAAAAABZg/p_TNCnMzZ7c/s800/april2008-3%20005.jpg)
Primer
![[Bild: april2008-3%20008.jpg]](https://lh5.ggpht.com/_W8gfKFqlA2E/SDclZcm8RwI/AAAAAAAABZ4/lLvlVk40FBc/s800/april2008-3%20008.jpg)
Base
Clear
![[Bild: cas%20039.jpg]](https://lh4.ggpht.com/_W8gfKFqlA2E/SH5fiSycSSI/AAAAAAAAB5k/dXamdygzirI/s800/cas%20039.jpg)
End result
![[Bild: cas%20027.jpg]](https://lh4.ggpht.com/_W8gfKFqlA2E/SH5eNlN75CI/AAAAAAAAB4g/Vby9NkiThy8/s800/cas%20027.jpg)
![[Bild: cas%20026.jpg]](https://lh5.ggpht.com/_W8gfKFqlA2E/SH5eMf69pSI/AAAAAAAAB4Y/L3n49nTHJ00/s800/cas%20026.jpg)
Okay, now the painter can give you a more precise price when the paint is removed, no more hidden repairs.
Sand with a eccentric rotary sander, with flex plate. WEAR A AAA QUALITY DUST MASK
You can try with a heat gun and razorblade
Sand layer by layer, don't dive in there and grind to the core,